断裂伸长率 | 500% | 拉伸强度 | 22MPa | 密度 | 0.951g/cm3 |
熔体流动速率 | 0.05g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
特性级别 | 高光泽 |
|
产品简述
断裂伸长率 | 500% | 拉伸强度 | 22MPa | 密度 | 0.951g/cm3 |
熔体流动速率 | 0.05g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
特性级别 | 高光泽 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | 23°C | ASTM D-1505/KS M3016 | 0.951 | g/cm3 | |
机械性能 | 撕裂强度 | MD | ASTM D-1922/KS M7016 | 22 | g | |
TD | ASTM D-1922/KS M7016 | 100 | g | |||
破裂点拉伸强力 | ASTM D-638/KS M3012 | 300 | kg/cm2 | |||
熔体流动速率 | ASTM D-1238/KS M3012 | 0.05 | g/10min | |||
破裂点张力 | MD | ASTM D-882/KS M3001 | 600 | kg/cm2 | ||
TD | ASTM D-882/KS M3001 | 580 | kg/cm2 | |||
屈服点拉伸强度 | ASTM D-638/KS M3012 | 230 | kg/cm2 | |||
破裂点断裂强度 | ASTM D-638/KS M3012 | >600 | % | |||
跌落冲击强度 | ASTM D-1709/KS A1028 | 150 | g | |||
断裂点伸张率 | MD | ASTM D-882/KS M3001 | 400 | % | ||
TD | ASTM D-882/KS M3001 | 500 | % |