| 断裂伸长率 | 343% | 拉伸强度 | 75MPa | 密度 | 0.952g/cm3 |
| 熔体流动速率 | 0.06g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
| 缺口冲击强度 | 300 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
|
|
产品简述
| 断裂伸长率 | 343% | 拉伸强度 | 75MPa | 密度 | 0.952g/cm3 |
| 熔体流动速率 | 0.06g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
| 缺口冲击强度 | 300 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 熔体流动速率 | ASTM D-1238 | 0.06 | g/10min | ||
| 熔体流动速率 | 190℃/21.6kg | ASTM D-1238 | 10 | g/10min | ||
| 密度 | 埃克森美孚法 | 0.952 | g/cm3 | |||
| 机械性能 | 屈服拉伸强度 | MD | ASTM D-882 | 37 | MPa | |
| TD | ASTM D-882 | 31 | MPa | |||
| 断裂拉伸强度 | MD | ASTM D-882 | 82 | MPa | ||
| TD | ASTM D-882 | 75 | MPa | |||
| 断裂伸长率 | MD | ASTM D-882 | 275 | % | ||
| TD | ASTM D-882 | 343 | % | |||
| 切割模量 | MD | 1% | ASTM D-882 | 993 | MPa | |
| TD | 1% | ASTM D-882 | 1060 | MPa | ||
| 落镖冲击强度 | F50 | ASTM D-1709A | 300 | g | ||
| 埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 9 | g | ||
| TD | ASTM D-1922 | 22 | g | |||
| 热性能 | 融化温度 | 埃克森美孚法 | 129 | ℃ | ||