断裂伸长率 | 700% | 拉伸强度 | 19MPa | 密度 | 0.925g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 110 |
|
产品简述
断裂伸长率 | 700% | 拉伸强度 | 19MPa | 密度 | 0.925g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 110 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.925 | g/cm3 | ||
熔体流动速率 | ISO 1133 | 2 | g/10min | |||
物理性能 | 光泽度 | 45℃ | ASTM D-2457 | 65 | units | |
摩擦系数 | ASTM D-1894 | 0.15-0.20 | ||||
机械性能 | 极限拉伸 | MD | ASTM D-882 | 20 | MPa | |
CD | ASTM D-882 | 19 | MPa | |||
Elmendorf断裂强度 | MD | ASTM D-1922 | 450 | g | ||
CD | ASTM D-1922 | 350 | g | |||
冲击强度 | ASTM D-1709 | 110 | g | |||
极限伸长率 | MD | ASTM D-882 | 450 | % | ||
TD | ASTM D-882 | 700 | % | |||
拉伸模量 | MD | ASTM D-882 | 190 | MPa | ||
CD | ASTM D-882 | 205 | MPa | |||
屈服拉伸 | MD | ASTM D-882 | 10 | MPa | ||
CD | ASTM D-882 | 11 | MPa | |||
热性能 | 维卡软化点 | ISO 306 | 96 | ℃ | ||
其它性能 | 混浊 | ASTM D-1003 | 8 | % |