断裂伸长率 | 720% | 拉伸强度 | 20.8MPa | 密度 | 0.923g/cm3 |
熔体流动速率 | 1.9g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 100 |
|
产品简述
断裂伸长率 | 720% | 拉伸强度 | 20.8MPa | 密度 | 0.923g/cm3 |
熔体流动速率 | 1.9g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 100 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.923 | g/cm3 | ||
熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 1.9 | g/10min | ||
薄膜厚度 | 50.8 | μ | ||||
机械性能 | 屈服拉伸强度 | MD | ASTM D-882 | 12.0 | MPa | |
TD | ASTM D-882 | 12.3 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 24.8 | MPa | ||
TD | ASTM D-882 | 20.8 | MPa | |||
断裂伸长率 | MD | ASTM D-882 | 520 | % | ||
TD | ASTM D-882 | 720 | % | |||
落镖冲击强度 | ASTM D-1709 | 100 | g | |||
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 560 | g | ||
TD | ASTM D-1922 | 470 | g | |||
热性能 | 维卡软化点 | ASTM D-1525 | 92.2 | ℃ | ||
熔点 | DSC | 111 | ℃ | |||
其它性能 | 薄膜强硬 | MD | ASTM D-882 | 184 | J/cm3 | |
TD | ASTM D-882 | 190 | J/cm3 | |||
光学性能 | 光泽度 | 45° | ASTM D-2457 | 70 | ||
雾度 | ASTM D-1003 | 7.5 | % |