断裂伸长率 | 700% | 拉伸强度 | 15MPa | 密度 | 0.923g/cm3 |
熔体流动速率 | 0.5g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 170 |
|
产品简述
断裂伸长率 | 700% | 拉伸强度 | 15MPa | 密度 | 0.923g/cm3 |
熔体流动速率 | 0.5g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 170 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.923 | g/cc | ||
熔体流动速率 | ASTM D-1238 | 0.5 | g/10min | |||
机械性能 | 断裂伸长率 | ASTM D-638 | 700 | % | ||
拉伸断裂强度 | MD | ASTM D-882 | 270 | kg/cm2 | ||
TD | ASTM D-882 | 230 | kg/cm2 | |||
断裂拉伸强度 | ASTM D-638 | 160 | kg/cm2 | |||
下降冲击强度 | ASTM D-1709 | 170 | g | |||
断裂伸长率 | MD | ASTM D-882 | 250 | % | ||
TD | ASTM D-882 | 600 | % | |||
拉伸抗热强度 | MD | ASTM D-1004 | 110 | kg/cm | ||
TD | ASTM D-1004 | 100 | kg/cm | |||
热性能 | 熔点 | ASTM D-2117 | 112 | ℃ | ||
维卡软化点 | ASTM D-1525 | 94 | ℃ | |||
其它性能 | 光泽度 | 45 | ASTM D-2457 | 60 | % | |
厚度 | HCC | 0.06 | ㎜ | |||
混浊度 | ASTM D-1009 | 18.0 | % |