断裂伸长率 | 620% | 拉伸强度 | 19.6MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2.3g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 96 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
|
产品简述
断裂伸长率 | 620% | 拉伸强度 | 19.6MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2.3g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 96 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.918 | g/cm3 | ||
熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 2.3 | g/10min | ||
薄膜厚度 | 50.8 | μ | ||||
机械性能 | 薄膜强度 | MD | ASTM D-882 | 140 | J/cm3 | |
TD | ASTM D-882 | 148 | J/cm3 | |||
切割模量 | MD | 2%正割 | ASTM D-882 | 166 | MPa | |
TD | 2%正割 | ASTM D-882 | 208 | MPa | ||
屈服拉伸强度 | MD | ASTM D-882 | 11.6 | MPa | ||
TD | ASTM D-882 | 11.0 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 21.8 | MPa | ||
TD | ASTM D-882 | 19.6 | MPa | |||
断裂伸长率 | MD | ASTM D-882 | 450 | % | ||
TD | ASTM D-882 | 620 | % | |||
落镖冲击强度 | ASTM D-1709 | 96 | g | |||
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 320 | g | ||
TD | ASTM D-1922 | 190 | g | |||
热性能 | 维卡软化点 | ASTM D-1525 | 92.2 | ℃ | ||
熔点 | DSC | 108 | ℃ | |||
光学性能 | 光泽度 | 45° | ASTM D-2457 | 40 | ||
雾度 | ASTM D-1003 | 16 | % |