断裂伸长率 | 530% | 拉伸强度 | 16MPa | 密度 | 0.925g/cm3 |
熔体流动速率 | 6.4g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 36 |
|
产品简述
断裂伸长率 | 530% | 拉伸强度 | 16MPa | 密度 | 0.925g/cm3 |
熔体流动速率 | 6.4g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 36 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.925 | g/cm3 | ||
熔体流动速率 | ASTM D-1338 | 6.4 | g/10min | |||
薄膜厚度 | 25.4 | μ | ||||
机械性能 | 屈服拉伸强度 | MD | ASTM D-882 | 13.9 | MPa | |
TD | ASTM D-882 | 12.8 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 25.1 | MPa | ||
TD | ASTM D-882 | 16.0 | MPa | |||
断裂伸长率 | MD | ASTM D-882 | 340 | % | ||
TD | ASTM D-882 | 530 | % | |||
落镖冲击强度 | ASTM D-1709 | 36 | g | |||
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 210 | g | ||
TD | ASTM D-1922 | 180 | g | |||
热性能 | 维卡软化点 | ASTM D-1525 | 96.1 | ℃ | ||
熔点 | DSC | 113 | ℃ | |||
其它性能 | 薄膜韧性 | MD | ASTM D-882 | 141 | J/cm3 | |
TD | ASTM D-882 | 132 | J/cm3 | |||
光学性能 | 光泽度 | 45° | ASTM D-2457 | 87 | ||
雾度 | ASTM D-1003 | 3.5 | % |