断裂伸长率 | 550% | 拉伸强度 | 21MPa | 密度 | 0.922g/cm3 |
熔体流动速率 | 3.5g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 130 |
|
产品简述
断裂伸长率 | 550% | 拉伸强度 | 21MPa | 密度 | 0.922g/cm3 |
熔体流动速率 | 3.5g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
缺口冲击强度 | 130 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 3.5 | g/10min | ||
密度 | 23℃ | ASTM D-1505 | 0.922 | g/cm3 | ||
机械性能 | 抗冲击强度 | ASTM D-1709 | 130 | g | ||
拉伸屈服强度 | MD | ASTM D-882 | 12 | MPa | ||
TD | ASTM D-882 | 10 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 19 | MPa | ||
TD | ASTM D-882 | 21 | MPa | |||
断裂伸长率 | MD | ASTM D-882 | 450 | % | ||
TD | ASTM D-882 | 550 | % | |||
热性能 | 维卡软化点 | ASTM D-1525 | 93 | ℃ | ||
晶体熔点 | ASTM E-794 | 109 | ℃ | |||
其它性能 | 摩擦系数 | ASTM D-1894 | 0.09 | |||
推荐薄膜厚度 | 20-100 | µm | ||||
透明度 | ASTM D-1746 | 70 | % | |||
雾度(浊度) | ASTM D-1003 | 8 | % | |||
光泽度 | ASTM D-2457 | 65 | gu |