断裂伸长率 | 200% | 拉伸强度 | 10.9MPa | 密度 | 0.924g/cm3 |
熔体流动速率 | 3g/10min | 用途级别 | 薄膜级 | 规格级别 | 吹塑 |
加工级别 | 吹塑级 |
|
产品简述
断裂伸长率 | 200% | 拉伸强度 | 10.9MPa | 密度 | 0.924g/cm3 |
熔体流动速率 | 3g/10min | 用途级别 | 薄膜级 | 规格级别 | 吹塑 |
加工级别 | 吹塑级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||||
基本性能 | 密度 | ASTM D-1505 | 0.924 | g/cm3 | ||||
熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 3 | g/10min | ||||
机械性能 | 薄膜厚度-Tested | 31.8 | um | |||||
割线模量-1% Secant | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
割线模量-1% Secant | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
拉伸屈服强度 | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
拉伸屈服强度 | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
拉抻断裂强度 | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
拉抻断裂强度 | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
拉伸断裂伸长率 | 31.8um,Blown Film | ASTM D-882 |
|
% | ||||
拉伸断裂伸长率 | 31.8um,Cast Film | ASTM D-882 |
|
% | ||||
落锤冲击 | 31.8um,Blown Film | ASTM D-1709 | 65 | g | ||||
落锤冲击 | 31.8um,Cast Film | ASTM D-1709 | 110 | g | ||||
埃尔曼多夫撕裂强度 | 31.8um,Blown Film | ASTM D-1922 |
|
g | ||||
埃尔曼多夫撕裂强度 | 31.8um,Cast Film | ASTM D-1922 |
|
g | ||||
光学性能 | 光泽度 | 45°,31.8um,Blown Film | ASTM D-2457 | 70 | ||||
光泽度 | 31.8um,Cast Film | ASTM D-2457 | 77 | |||||
雾度 | 31.7um,Blown Film | ASTM D-1003 | 5.4 | % | ||||
雾度 | 31.7um,Cast Film | ASTM D-1003 | 3.4 | % |