断裂伸长率 | 800% | 拉伸强度 | 32MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
加工级别 | 吹塑级 |
|
产品简述
断裂伸长率 | 800% | 拉伸强度 | 32MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
加工级别 | 吹塑级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.918 | g/cm3 | ||
熔体流动速率 | ASTM D-1238 | 1.0 | g/10min | |||
物理性能 | 光泽度 | 60℃ | ASTM D-2457 | 60 | ||
机械性能 | 断裂伸长率 | MD | ASTM D-882 | 750 | % | |
TD | ASTM D-882 | 800 | % | |||
Elmendorf断裂强度 | MD | ASTM D-1922 | 165 | g | ||
TD | ASTM D-1922 | 300 | g | |||
Puncture resistance | SABIC | 68 | J/mm | |||
1%割线模量 | MD | ASTM D-882 | 220 | MPa | ||
TD | ASTM D-882 | 260 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 40 | MPa | ||
TD | ASTM D-882 | 32 | MPa | |||
Dart冲击强度 | ASTM D-1709 | 154 | g | |||
屈服拉伸强度 | MD | ASTM D-882 | 11 | MPa | ||
TD | ASTM D-882 | 11.5 | MPa | |||
其它性能 | 混浊 | ASTM D-1003 | 9.5 | % |