断裂伸长率 | 714% | 拉伸强度 | 25MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 维卡软化点 | 101℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 714% | 拉伸强度 | 25MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 维卡软化点 | 101℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.9180 | g/cc | ||
机械性能 | 断裂拉伸强度 | MD | ASTM D-882 | 31.7 | MPa | |
TD | ASTM D-882 | 25.1 | MPa | |||
屈服拉伸强度 | MD | ASTM D-882 | 10.3 | MPa | ||
TD | ASTM D-882 | 11.1 | MPa | |||
Dart 冲击强度 | ASTM D-1709 | <100 | g | |||
刺穿强度 | ASTM DOW | 8.2 | J/cm3 | |||
热性能 | 维卡软化点 | ASTM D-1525 | 101 | ℃ | ||
其它性能 | 断裂伸长率 | MD | ASTM D-882 | 658 | % | |
TD | ASTM D-882 | 714 | % | |||
熔点 | ASTM DOW | 108 | ℃ | |||
抗撕裂性 | MD | ASTM D-1992 | 106 | g | ||
TD | ASTM D-1992 | 256 | g | |||
韧性 | MD | ASTM D-882 | 102.6 | J/cm3 | ||
TD | ASTM D-882 | 98.1 | J/cm3 | |||
熔融指数 | ASTM D-1238 | 1.00 | g/10min | |||
透明度 | ASTM D-1746 | 97 | ||||
拉伸模量 | MD | ASTM D-882 | 183.3 | MPa | ||
TD | ASTM D-882 | 217.4 | MPa | |||
光泽度 | ASTM D-2457 | 76 | ||||
雾度 | ASTM D-1003 | 7.8 | % |