断裂伸长率 | 682% | 拉伸强度 | 21MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2g/10min | 维卡软化点 | 96℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 682% | 拉伸强度 | 21MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2g/10min | 维卡软化点 | 96℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-792 | 0.9180 | g/cc | ||
机械性能 | 屈服拉伸强度 | MD | ASTM D-882 | 11 | MPa | |
TD | ASTM D-882 | 9 | MPa | |||
断裂拉伸强度 | MD | ASTM D-882 | 40 | MPa | ||
TD | ASTM D-882 | 21 | MPa | |||
Dart 冲击强度 | ASTM D-1709 | 66 | g | |||
刺穿强度 | ASTM DOW | 9 | J/cm3 | |||
热性能 | 维卡软化点 | ASTM D-1525 | 96 | ℃ | ||
其它性能 | 断裂伸长率 | MD | ASTM D-882 | 447 | % | |
TD | ASTM D-882 | 682 | % | |||
熔融指数 | ASTM D-1238 | 2.0 | g/10min | |||
雾度 | ASTM D-1003 | 0.56 | % | |||
光泽度 | ASTM D-2457 | 151 | ||||
抗撕裂性 | MD | ASTM D-1992 | 37 | g | ||
TD | ASTM D-1992 | 370 | g | |||
拉伸模量 | MD | ASTM D-882 | 149 | MPa | ||
TD | ASTM D-882 | 147 | MPa | |||
透明度 | ASTM D-1746 | 99 | ||||
熔点 | ASTM DOW | 104 | ℃ |