断裂伸长率 | 810% | 拉伸强度 | 44MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 维卡软化点 | 93℃ | 用途级别 | 薄膜级,食品级,光学级 |
规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 810% | 拉伸强度 | 44MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 1g/10min | 维卡软化点 | 93℃ | 用途级别 | 薄膜级,食品级,光学级 |
规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 1.0 | g/10min | ||
密度 | ASTM D-1505 | 0.918 | g/cm3 | |||
机械性能 | 拉力断裂伸长率 | MD | ASTM D-882B | 620 | % | |
TD | ASTM D-882B | 810 | % | |||
落球冲击强度 | ASTM D-1709 | 610 | g | |||
拉力断裂强度 | MD | ASTM D-882B | 500 | kg/cm2 | ||
TD | ASTM D-882B | 450 | kg/cm2 | |||
拉力降伏强度 | MD | ASTM D-882B | 100 | kg/cm2 | ||
TD | ASTM D-882B | 110 | kg/cm2 | |||
1%伸长弹性系数 | MD | ASTM D-882B | 1600 | kg/cm2 | ||
TD | ASTM D-882B | 2000 | kg/cm2 | |||
抗撕裂性 | MD | ASTM D-1922 | 305 | g/25µm | ||
TD | ASTM D-1922 | 500 | g/25µm | |||
热性能 | 软化点 | ASTM D-1525 | 93 | ℃ | ||
熔点 | DSC | 121 | ℃ | |||
脆化温度 | ASTM D-746 | <-70 | ℃ | |||
其它性能 | 光泽度 | 45℃ | ASTM D-2457 | 51 | % | |
浊度 | ASTM D-1003 | 15 | % | |||
滑剂 | 高 | |||||
抗粘剂 | 高 | |||||
透明度 | 60 | % |