断裂伸长率 | 750% | 拉伸强度 | 36MPa | 密度 | 0.926g/cm3 |
熔体流动速率 | 0.7g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 750% | 拉伸强度 | 36MPa | 密度 | 0.926g/cm3 |
熔体流动速率 | 0.7g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 0.7 | g/10min | ||
密度 | ASTM D-792 | 0.926 | g/cm3 | |||
物理性能 | 光泽度 | 60℃ | ASTM D-2457 | 85 | ||
机械性能 | 断裂伸长率 | MD | ASTM D-882 | 600 | % | |
TD | ASTM D-882 | 750 | % | |||
门氏撕裂强度 | MD | ASTM D-1922 | 140 | g | ||
TD | ASTM D-1922 | 450 | g | |||
1%割线模量 | MD | ASTM D-882 | 270 | MPa | ||
TD | ASTM D-882 | 285 | MPa | |||
落锤冲击 | F50 | ASTM D-1709 | 140 | g | ||
抗穿刺强度 | SABIC | 62 | J/mm | |||
断裂拉伸强度 | MD | ASTM D-882 | 44 | MPa | ||
TD | ASTM D-882 | 36 | MPa | |||
屈服拉伸强度 | MD | ASTM D-882 | 12 | MPa | ||
TD | ASTM D-882 | 13 | MPa | |||
其它性能 | 混浊 | ASTM D-1003 | 8.5 | % |