断裂伸长率 | 750% | 拉伸强度 | 27MPa | 密度 | 0.919g/cm3 |
熔体流动速率 | 2.8g/10min | 维卡软化点 | 100℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 750% | 拉伸强度 | 27MPa | 密度 | 0.919g/cm3 |
熔体流动速率 | 2.8g/10min | 维卡软化点 | 100℃ | 用途级别 | 薄膜级 |
规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
熔体流动速率 | ASTM D-1238 | 2.8 | g/10min | |||
物理性能 | 薄膜厚度 | ASTM D-746 | 25 | µm | ||
机械性能 | 断裂伸长率 | MD | ASTM D-882 | 650 | % | |
TD | ASTM D-882 | 750 | % | |||
撕裂弹性率 | MD | ASTM D-882 | 2800 | Kg/cm2 | ||
TD | ASTM D-882 | 2800 | Kg/cm2 | |||
撕裂强度 | MD | ASTM D-1004 | 115 | Kg/cm | ||
TD | ASTM D-1004 | 105 | Kg/cm | |||
尖头冲击强度 | ASTM D-3420 | 3.5 | g/μm | |||
拉伸屈服强度 | MD | ASTM D-882 | 120 | Kg/cm2 | ||
TD | ASTM D-882 | 110 | Kg/cm2 | |||
拉伸断裂强度 | MD | ASTM D-882 | 300 | Kg/cm2 | ||
TD | ASTM D-882 | 280 | Kg/cm2 | |||
热性能 | 低温脆化温度 | ASTM D-746 | <-70 | ℃ | ||
维卡软化点 | ASTM D-1525 | 100 | ℃ |