详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 密度 | ASTM D-792 | 0.932 | g/cm3 | |
熔体流动速率 | 190℃/2.16 kg | ASTM D-1238 | 0.5 | g/10min | |
厚度 | 20.3 | microns | |||
粘连性 | 3500 | ppm | |||
爽滑性 | 1200 | ppm | |||
机械性能 | 拉伸屈服强度 | MD | ASTM D-882 | 25.1 | MPa |
拉伸屈服强度 | TD | ASTM D-882 | 25.8 | MPa | |
断裂伸长率 | MD | ASTM D-882 | 530 | % | |
断裂伸长率 | TD | ASTM D-882 | 716 | % | |
冲击强度 | TD | ASTM D-882 | 4414 | ||
冲击强度 | MD | ASTM D-882 | 5723 | ||
割线模量 | MD,2% | ASTM D-882 | 0.299805 | GPa | |
割线模量 | TD,2% | ASTM D-882 | 0.315559 | GPa | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 332 | g | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 599 | g | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 16.3 | g/micron | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 29.5 | g/micron | |
落锤冲击 | Method B | ASTM D-1709 | Max100 | g | |
落锤冲击 | Method A | ASTM D-1709 | 126 | g | |
拉伸断裂强度 | MD | ASTM D-882 | 78.4 | MPa | |
拉伸断裂强度 | TD | ASTM D-882 | 75.5 | MPa | |
热封强度 | Dow Method | 12.9 | N | ||
热性能 | 热封强度始封温度 | Dow Method | 120 | ℃ | |
熔点 | 126 | ℃ | |||
维卡软化点 | 119 | ℃ | |||
光学性能 | 雾度 | 13 | % | ||
光泽度 | 20 ° | 46 | % | ||
光泽度 | 45 ° | 49 | % |