用途级别 | 薄膜级 | 规格级别 | 薄膜吹塑 | 加工级别 | 吹塑级 |
|
产品简述
用途级别 | 薄膜级 | 规格级别 | 薄膜吹塑 | 加工级别 | 吹塑级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 密度 | ASTM D-792 | 0.9289 | g/cm3 | |
熔体流动速率 | 190℃/2.16 kg | ASTM D-1238 | 0.8 | g/10min | |
厚度 | 20.3 | microns | |||
粘连性 | 4000 | ppm | |||
机械性能 | 拉伸屈服强度 | MD | ASTM D-882 | 16.6 | MPa |
拉伸屈服强度 | TD | ASTM D-882 | 19.6 | MPa | |
断裂伸长率 | MD | ASTM D-882 | 703 | % | |
断裂伸长率 | TD | ASTM D-882 | 793 | % | |
冲击强度 | TD | ASTM D-882 | 3701 | ||
冲击强度 | MD | ASTM D-882 | 4832 | ||
割线模量 | MD,2% | ASTM D-882 | 0.298577 | GPa | |
割线模量 | TD,2% | ASTM D-882 | 0.282975 | GPa | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 171 | g | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 715 | g | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 8.42 | g/micron | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 35.2 | g/micron | |
落锤冲击 | Method B | ASTM D-1709 | Max100 | g | |
落锤冲击 | Method A | ASTM D-1709 | 55 | g | |
拉伸断裂强度 | MD | ASTM D-882 | 48.5 | MPa | |
拉伸断裂强度 | TD | ASTM D-882 | 54 | MPa | |
热封强度 | Dow Method | 13.3 | N | ||
热性能 | 热封强度始封温度 | Dow Method | 120 | ℃ | |
熔点 | 126 | ℃ | |||
维卡软化点 | 116 | ℃ | |||
光学性能 | 雾度 | 9 | % | ||
光泽度 | 20 ° | 73 | % | ||
光泽度 | 45 ° | 77 | % |