加工级别 | 注塑级 |
|
产品简述
加工级别 | 注塑级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 密度 | ASTM D-792 | 0.925 | g/cm3 | |
熔体流动速率 | ASTM D-1238 | 0.8 | g/10min | ||
厚度 | 38.1 | microns | |||
抗粘连剂 | 4500 | ppm | |||
滑爽剂 | 1000 | ppm | |||
机械性能 | 落锤 | ASTM D-1709 | 4.53 | g/micron | |
拉伸屈服强度 | ASTM D-882 | 13 | MPa | ||
拉伸屈服强度 | ASTM D-882 | 15 | MPa | ||
1%割线模量 | ASTM D-882 | 0.286 | GPa | ||
1%割线模量 | ASTM D-882 | 0.347 | GPa | ||
断裂伸长率 | MD | ASTM D-882 | 610 | % | |
断裂伸长率 | TD | ASTM D-882 | 710 | % | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 7.09 | g | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 24.8 | g | |
拉伸断裂强度 | MD | ASTM D-882 | 55.5 | MPa | |
拉伸断裂强度 | TD | ASTM D-882 | 45 | MPa | |
热性能 | 熔点 | 125 | ℃ | ||
光学性能 | 雾度 | ASTM D-1003 | 15 | % | |
光泽度 | ASTM D-2457 | 50 | % |