断裂伸长率 | 830% | 拉伸强度 | 33MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
|
产品简述
断裂伸长率 | 830% | 拉伸强度 | 33MPa | 密度 | 0.918g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 2.0 | g/10min | ||
密度 | ExxonMobil Method | 0.918 | g/cm3 | |||
机械性能 | 极限伸长率 | MD | ASTM D-882 | 700 | % | |
TD | ASTM D-882 | 830 | % | |||
Elmendorf断裂强度 | MD | ASTM D-1922 | 150 | g | ||
TD | ASTM D-1922 | 340 | g | |||
断裂拉伸强度 | MD | ASTM D-882 | 5800 | psi(MPa) | ||
TD | ASTM D-882 | 4800 | psi(MPa) | |||
热性能 | 熔点 | ExxonMobil Method | 249(121) | ℉(℃) | ||
其它性能 | 击穿 | ExxonMobil Method | 20 | in.lb | ||
计量 | ASTM D-374 | 1.2 | mil | |||
1%割线模量 | MD | ASTM D-882 | 28 | psi(MPa) | ||
TD | ASTM D-882 | 33 | psi(MPa) | |||
混浊度 | ASTM D-1003 | 18 | % | |||
屈服拉伸强度 | MD | ASTM D-882 | 1400 | psi(MPa) | ||
TD | ASTM D-882 | 1400 | psi(MPa) | |||
光泽度 | ASTM D-2457 | 40 |