性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 密度 | ASTM D-792 | 0.917 | g/cm3 | |
熔体流动速率 | 190℃/2.16 kg | ASTM D-1238 | 2 | g/10min | |
厚度 | 20.3 | microns | |||
机械性能 | 落锤 | ASTM D-1709 | 4.45 | g/micron | |
拉伸屈服强度 | ASTM D-882 | 8.3 | MPa | ||
拉伸屈服强度 | ASTM D-882 | 7.6 | MPa | ||
割线模量 | ASTM D-882 | 0.117 | GPa | ||
割线模量 | ASTM D-882 | 0.131 | GPa | ||
断裂伸长率 | MD | ASTM D-882 | 410 | % | |
断裂伸长率 | TD | ASTM D-882 | 820 | % | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 160 | g | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 920 | g | |
拉伸断裂强度 | MD | ASTM D-882 | 69 | MPa | |
拉伸断裂强度 | TD | ASTM D-882 | 36.5 | MPa | |
埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 7.87 | g/micron | |
埃尔曼多夫撕裂强度 | TD | ASTM D-1922 | 45.3 | g/micron | |
热性能 | 熔点 | 124 | ℃ | ||
光学性能 | 雾度 | ASTM D-1003 | 2 | % | |
光泽度 | ASTM D-2457 | 95 | % |