断裂伸长率 | 750% | 拉伸强度 | 29MPa | 密度 | 0.92g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
脆化温度 | -70℃ | 加工级别 | 吹塑级 |
|
产品简述
断裂伸长率 | 750% | 拉伸强度 | 29MPa | 密度 | 0.92g/cm3 |
熔体流动速率 | 2g/10min | 用途级别 | 薄膜级 | 规格级别 | 薄膜 |
脆化温度 | -70℃ | 加工级别 | 吹塑级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.920 | g/cm3 | ||
熔体流动速率 | ASTM D-1238 | 2.00 | g/10min | |||
物理性能 | 光泽度 | 45℃ | ASTM D-2457 | 60 | ||
薄膜厚度 | HYUNDAI | 30 | um | |||
机械性能 | 落球冲击强度 | ASTM D-1709 | 50 | g | ||
撕裂伸长率 | MD | ASTM D-882 | 650 | % | ||
TD | ASTM D-882 | 750 | % | |||
撕裂强度 | MD | TEAR LENGTH 21.5mm | ASTM D-1992 | 30 | % | |
TD | TEAR LENGTH 21.5mm | ASTM D-1992 | 140 | % | ||
撕裂拉伸强度 | MD | ASTM D-882 | 400 | kg/cm2 | ||
TD | ASTM D-882 | 300 | kg/cm2 | |||
热性能 | 低温脆点 | ASTM D-746 | <-70 | ℃ |