性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
成型收缩率 | UBEmethod | 1.5 | % | |
吸水率 | ASTM D-570 | 1.8 | % | |
成型收缩率 | UBEmethod | 1.4 | % | |
吸水率 | ASTM D-570 | 10.7 | % | |
比重 | ASTM D-792 | 1.14 | ||
TABER磨耗率 | ASTM D-1044 | 7 | mg | |
屈服下的伸张强度 | 23° | ASTM D-638 | 400 | kgf/cm2 |
弯曲强度 | -30° | ASTM D-790 | 1300 | kgf/cm2 |
挤剪强度 | 23° | ASTM D-732 | 600 | kgf/cm2 |
屈服下的伸张强度 | 80° | ASTM D-638 | 320 | kgf/cm2 |
弯曲弹性率 | 80° | ASTM D-790 | 7000 | kgf/cm2 |
断裂下的伸张强度 | 23° | ASTM D-638 | 650 | kgf/cm2 |
屈服下的伸张强度 | -30° | ASTM D-638 | 870 | kgf/cm2 |
弯曲弹性率 | 23° | ASTM D-790 | 7500 | kgf/cm2 |
屈服下的延伸率 | 23° | ASTM D-638 | 8 | % |
弯曲弹性率 | 80° | ASTM D-790 | 4000 | kgf/cm2 |
弯曲弹性率 | -30° | ASTM D-790 | 36000 | kgf/cm2 |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 85 | |
弯曲强度 | 23° | ASTM D-790 | 400 | kgf/cm2 |
抗冲击强度 | 23° | ASTM D-256 | 50 | kgf.cm/cm |
屈服下的伸张强度 | 80° | ASTM D-638 | 180 | kgf/cm2 |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 55 | |
抗冲击强度 | -30° | ASTM D-256 | 4.0 | kgf.cm/cm |
弯曲强度 | 80° | ASTM D-790 | 250 | kgf/cm2 |
弯曲强度 | 23° | ASTM D-790 | 1100 | kgf/cm2 |
屈服下的伸张强度 | -30° | ASTM D-638 | 1100 | kgf/cm2 |
硬度(洛氏、布氏) | 23° | ASTM D-785 | 120 | |
弯曲弹性率 | 23° | ASTM D-790 | 26000 | kgf/cm2 |
弯曲弹性率 | -30° | ASTM D-790 | 34000 | kgf/cm2 |
断裂下的延伸率 | 23° | ASTM D-638 | 170 | % |
1%变形下的压缩强度 | 23° | ASTM D-695 | 200 | kgf/cm2 |
屈服下的伸张强度 | 23° | ASTM D-638 | 750 | kgf/cm2 |
弯曲强度 | -30° | ASTM D-790 | 1400 | kgf/cm2 |
抗冲击强度 | 23° | ASTM D-256 | 6.0 | kgf.cm/cm |
挤剪强度 | 23° | ASTM D-732 | 650 | kgf/cm2 |
断裂下的延伸率 | 23° | ASTM D-638 | >200 | % |
1%变形下的压缩强度 | 23° | ASTM D-695 | 100 | kgf/cm2 |
弯曲强度 | 80° | ASTM D-790 | 400 | kgf/cm2 |
介电常数 | 103HZ | ASTM D-150 | 3.8 | |
绝缘耐力 | KV/mm | ASTM D-149 | 20 | |
介电常数 | 106HZ | ASTM D-150 | 4.5 | |
介电常数 | 60HZ | ASTM D-150 | 3.9 | |
介电常数 | 106HZ | ASTM D-150 | 3.5 | |
抗电弧强度 | ASTM D-495 | 119 | S | |
介电损耗 | 60HZ | ASTM D-150 | 0.10 | |
介电常数 | 60HZ | ASTM D-150 | 9.0 | |
介电损耗 | 103HZ | ASTM D-150 | 0.02 | |
介电损耗 | 103HZ | ASTM D-150 | 0.10 | |
介电损耗 | 60HZ | ASTM D-150 | 0.01 | |
体积电阻率 | ASTM D-257 | 1012 | Ω.cm | |
IEC电路 | UL746 | 600+ | V | |
介电损耗 | 106HZ | ASTM D-150 | 0.02 | |
介电损耗 | 106HZ | ASTM D-150 | 0.12 | |
体积电阻率 | ASTM D-257 | 1015 | Ω.cm | |
介电常数 | 103HZ | ASTM D-150 | 8.0 | |
热变形温度 | 4.6kgf/cm2 | ASTM D-648 | 175 | °C |
熔点 | DSC | 215-225 | °C | |
热变形温度 | 18.6kgf/cm2 | ASTM D-648 | 75 | °C |
线性热膨胀系数 | ASTM D-696 | 8 | X的10-5cm/cm/°C | |
燃烧率 | UL94 | V-2 |