密度 | 1.5g/cm3 | 吸水率 | 0.06% | 硬度 | 119 |
规格级别 | 玻纤增强 | 特性级别 | 增强级,阻燃级 |
|
产品简述
密度 | 1.5g/cm3 | 吸水率 | 0.06% | 硬度 | 119 |
规格级别 | 玻纤增强 | 特性级别 | 增强级,阻燃级 |
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
物理性能 | 比重 | 固体 | ASTM D-792 | 1.50 | --- | |
比容 | --- | ASTM D-792 | 18.50 | in3/lb | ||
吸水率 | 24 小时 @ 73F | ASTM D-570 | 0.060 | % | ||
模塑收缩量 | 60-125 mil | flow | ASTM D-955 | 3-5 | in/in E-3 | |
125-180 mil | flow | ASTM D-955 | 5-8 | in/in E-3 | ||
60-125 mil | xflow | ASTM D-955 | 4-6 | in/in E-3 | ||
125-180 mil | xflow | ASTM D-955 | 6-9 | in/in E-3 | ||
机械性能 | 仪表控制抗冲击能量 | @ 峰值, 73F | ASTM D-3763 | 5.0 | ft-lbs | |
挠曲模量 | --- | ASTM D-790 | 1000000 | psi | ||
伊佐德冲击值 | 无缺口 | 73F | ASTM D-4812 | 12.0 | ft-lb/in | |
缺口 | 73F | ASTM D-256 | 1.8 | ft-lb/in | ||
缺口 | -22F | ASTM D-256 | 1.5 | ft-lb/in | ||
挠曲强度 | 断裂 | ASTM D-790 | 27500 | psi | ||
抗拉强度 | 断裂 | ASTM D-638 | 16000 | psi | ||
压缩强度 | --- | ASTM D-695 | 16700 | psi | ||
洛氏硬度 | --- | ASTM D-785 | 119 | R | ||
剪切强度 | --- | ASTM D-732 | 8260 | psi | ||
仪表控制抗冲击总能量 | 73F | ASTM D-3763 | 6.0 | ft-lbs | ||
电气性能 | 介电常数 | 100 Hz | -- | ASTM D-150 | 3.60 | -- |
1 MHz | -- | ASTM D-150 | 3.60 | -- | ||
体积电阻率 | --- | ASTM D-257 | 5E16 | ohm-cm | ||
损耗因数 | 100 Hz | -- | ASTM D-150 | 0.0014 | -- | |
1 MHz | -- | ASTM D-150 | 0.0200 | -- | ||
介电强度 | 125 mils | 空气中 | ASTM D-149 | 600 | V/mil | |
62 mils | 油内 | ASTM D-149 | 740 | V/mil | ||
热性能 | 热指数 | 电性能 | --- | UL 746B | 125 | deg C |
机械冲击性能 | --- | UL 746B | 110 | deg C | ||
非机械冲击性能 | --- | UL 746B | 125 | deg C | ||
CTE(热膨胀系数) | ASTM E-831 | flow | -40F ~ 100F | 1 E-5 | in/in-F | |
ASTM E-831 | flow | 140F ~ 280F | 0 E-5 | in/in-F | ||
HDT(热畸变温度) | 未退火 | 66 psi | ASTM D-648 | 420 | deg F | |
未退火 | 264 psi | ASTM D-648 | 350 | deg F | ||
其它性能 | 额定HB值 (测试厚度) | --- | UL 94 | 0.058 | inch | |
UL 文件号, 美国 | --- | --- | E121562 | --- |