规格级别 | 玻纤增强 | 加工级别 | 注塑级 | 特性级别 | 增强级,抗紫外线 |
|
产品简述
规格级别 | 玻纤增强 | 加工级别 | 注塑级 | 特性级别 | 增强级,抗紫外线 |
备注:特性:玻纤增强20%
详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 吸水率 | ASTM D-570 | 0.16 | % | |
模具收缩率 | 3.2mm | ASTM D-955 | 1-3 | 10-3 | |
物理性能 | 阻燃性 | --- | UL 94 | 3.2 | mm |
增强 | --- | --- | 20 | % | |
阻燃性 | --- | UL 94 | 5V | --- | |
弯曲模量 | --- | ASTM D-790 | 5512 | MPa | |
阻燃性 | --- | UL 94 | 1.5 | mm | |
比重 | ASTM D-792 | 1.35 | --- | ||
阻燃性 | --- | UL 94 | V-1 | --- | |
机械性能 | 缺口冲击强度 | 23℃ | ASTM D-256 | 107 | J/m |
洛氏硬度 | --- | ASTM D-785 | 122 | --- | |
弯曲强度 | --- | ASTM D-790 | 131 | MPa | |
断裂伸长率 | --- | ASTM D-638 | 5 | % | |
拉伸强度 | --- | ASTM D-638 | 110 | MPa | |
电气性能 | 损耗因数 | 60Hz | ASTM D-150 | 0.0009 | --- |
体积电阻率 | --- | ASTM D-257 | 1.0×1017 | Ω.cm | |
介电常数 | 60Hz | ASTM D-150 | 3.17 | --- | |
损耗因数 | 1MHz | ASTM D-150 | 0.0073 | --- | |
介电常数 | 1MHz | ASTM D-150 | 3.13 | --- | |
热性能 | 热变形温度 | 0.45MPa | ASTM D-648 | 148 | ℃ |