详细数据
订购指南
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 密度 | ExxonMobil Method | 0.882 | g/cm3 | |
雾度2 | ASTM D-1003 | 13@50mils | % | ||
熔融指数 | ASTM D-1238 | 10.0 | g/10 min | ||
熔体流动速率 | ASTM D-1238 | 25 | g/10 min | ||
硬度2 | Shore D,15 sec | ASTM D-2240 | 27 | ||
硬度2 | Shore A,15 sec | ASTM D-2240 | 79 | ||
物理性能 | 拉伸强度3 | @Break | ASTM D-638 | No Break | psi(MPa) |
缺口冲击强度 | -40℃ | ASTM D-256 | No Break | ft-lb/in(J/m) | |
弯曲模量 | 1% secant | ASTM D-790 | 3807(26.2) | psi(MPa) | |
缺口冲击强度 | 23℃ | ASTM D-256 | No Break | ft-lb/in(J/m) | |
拉伸率 | @Break | ASTM D-638 | No Break | % | |
热性能 | 最高熔体温度 | ExxonMobil Method | 164.7(73.7) | ℉(℃) | |
维卡软化点2 | 200g | ASTM D-1525 | 159.8(71.0) | ℉(℃) | |
其它性能 | 拉伸应力5 | @100% Elongation | ASTM D-412 | 407(2.8) | psi(MPa) |
拉伸应力5 | @300% Elongation | ASTM D-412 | 493(3.4) | psi(MPa) | |
门尼粘度ML(1+4) | 125℃ | ASTM D-1646 | 5.9 | Torgue Units | |
抗扯强度 | ASTM D-624 | 245.9(43.1) | lb/in(kN/m) | ||
拉伸率 | @Break | ASTM D-412 | No Break | % |